How a thermal shrinkage of 1-2% is measured: the condition matters more than the number

A thermal shrinkage figure means nothing once the temperature, the duration and the atmosphere are stripped away. This article reads a figure through the GB/T 36363-2018 basis, explains the difference between the machine and cross directions, and separates it from the breakdown temperature, which is an independent measurement.

01

The note

Figures are quoted with their test condition and standard; project-specific data is confirmed one to one at the sample stage.

A figure has to arrive with its conditions

Thermal shrinkage is a conditional property. Temperature, duration, atmosphere, specimen size and orientation together determine the result. The behaviour of one material in a 130 °C / 1 h window and in a 180 °C / 0.5 h window cannot be used interchangeably, so the condition has to travel with the number.

For this company's products the published basis is fixed at 180 °C / 30 min in an air atmosphere, giving 1-2% for both the machine and cross directions under GB/T 36363-2018, with the report conclusion stated as thermal shrinkage performance ≤3%. The value of a fixed basis is that every batch and every model can be compared against the same ruler.

Why both directions are reported

A film carries orientation from forming and coating, so the machine (MD) and transverse (TD) shrinkage are rarely identical. Reporting one direction alone invites the reader to assume the other is necessarily smaller or larger, when in practice they are close but not equal.

The acceptance basis requires both directions to fall inside the interval rather than taking the better side. The convention is stricter than single-direction acceptance, and it matches the practical constraint: dimensional stability has to hold in both directions.

Shrinkage and breakdown temperature are different measurements

Thermal shrinkage answers how much the dimensions changed. The breakdown temperature answers at what temperature an obvious dimensional change appears. They come from different tests, they are not two names for the same indicator, and one cannot be converted into the other.

The breakdown condition is a nitrogen atmosphere, 100 °C/min heating and 0.02 N tension (GB/T 36800-2018). The company's figure is above 400 °C: dimensions remain almost unchanged from room temperature up to and beyond 400 °C, with an obvious change appearing above that point. The test was carried out by the Waters Technologies application laboratory of TA Instruments.

When both figures are quoted, it is worth stating what question each one answers. Saying only 'high temperature resistant' without the conditions gives the reader nothing that can be checked.

Using the basis in an actual selection

A practical method is to write down the temperature and duration ceiling the cell can realistically experience, and then look for data with an explicit acceptance condition in that window. A percentage offered without conditions should not enter the decision at all.

The same logic applies to the breakdown temperature. If the thermal failure path of the cell is already constrained by other design measures, then mechanical retention within the heat treatment window is a more productive discussion than comparing breakdown temperatures as isolated highlights.

02

Related pages

To discuss a parameter range for a specific cell architecture, contact the technical team directly.