Insights / Technical notes

The parts of separator
selection that stay vague

Every note starts from a real question on the cell side and sets out the order of checks, the test conditions and the conclusions that can be verified. Every figure quoted comes with its condition and method.

01

All notes

The notes are compiled from company measurements and published standards. Project-specific data is confirmed one to one during the sample stage.

Test conditions

How a thermal shrinkage of 1-2% is measured: the condition matters more than the number

A thermal shrinkage figure means nothing once the temperature, the duration and the atmosphere are stripped away. This article reads a figure through the GB/T 36363-2018 basis, explains the difference between the machine and cross directions, and separates it from the breakdown temperature, which is an independent measurement.

Safety boundaries

What a breakdown temperature above 400 °C does and does not say

The breakdown temperature is a material-level property of a separator, and the separator does more in a cell than provide one barrier. This article sets out what the figure can support, what it cannot, and which parts of a cell safety assessment remain outside it.

Material behaviour

Does puncture strength drop after aramid coating? Read the heat window first

A common worry is that adding a coating to the separator surface weakens it mechanically. This article reports the measured results for the ranges below 145 °C, 150 °C / 0.5 h and 180 °C / 0.5 h, and explains why the retention ratio and the absolute value have to be read separately.

Process difficulty

Where the difficulty of aramid coating actually lies: four requirements that pull in opposite directions

The process itself is a company trade secret and is not published, but the reasons behind the difficulty can be discussed: heat resistance and wetting pull in opposite directions, mechanical strength is a curve against temperature, the thickness budget narrows the scheme space, and batch consistency is harder than a single-batch peak. This article explains those four and gives five checkable actions for selection and verification.

Interface and wetting

Adhesion and wetting are two different questions: their criteria and how to read them together

Adhesion between separator and electrode, and wetting of the separator by electrolyte, are independent problems with different criteria, different methods and different failure modes. This article gives the criterion on the adhesion side (peel strength >30 N/m, GB/T 7122-96) and the criteria on the wetting side (porosity about 35%-45%, air permeability 226-366 s), explains why they must be read together, and points out a common misreading of the measurement basis.