Adhesion between separator and electrode, and wetting of the separator by electrolyte, are independent problems with different criteria, different methods and different failure modes. This article gives the criterion on the adhesion side (peel strength >30 N/m, GB/T 7122-96) and the criteria on the wetting side (porosity about 35%-45%, air permeability 226-366 s), explains why they must be read together, and points out a common misreading of the measurement basis.

01

The note

Figures are quoted with their test condition and standard; project-specific data is confirmed one to one at the sample stage.

Two interface questions that are often conflated

The **adhesion** between separator and electrode, and the **wetting** of the separator by electrolyte, are independent questions, yet they are often merged into a single vague claim about interface performance.

Adhesion answers whether the electrode and separator stay bonded through assembly and thermal treatment. Wetting answers whether the electrolyte can enter, spread and be retained.

Their criteria differ, their measurement methods differ, and they fail in different ways. Talking about them separately is what makes the criteria checkable.

The adhesion criterion: peel strength and its acceptance basis

Adhesion is quantified by peel strength, measured under GB/T 7122-96 (Determination of peel strength of high-strength adhesives, floating roller method). The company **internal acceptance criterion** is >30 N/m.

Test data show that both the single-side and the double-side coated schemes meet that criterion, and that the double-side scheme meets it stably across a wider range of process conditions.

The acceptance threshold and the measured value must be kept apart here. The former is the promise the company makes; the latter is the number on each batch report. Use the threshold to compare suppliers side by side and the measured value to trace a batch back through time. The two cannot be mixed, and a measured value should not be used to back out a claimed lower bound.

The wetting criteria: porosity and air permeability

On the wetting side the quantified figures are the porosity of the separator as a whole and its air permeability in Gurley seconds. Measured across multiple coated batches, the separator porosity as a whole is about 35%-45%, the porosity of the aramid coating mostly falls in the 50%-71% band, and air permeability is about 226-366 s. The basis standard is GB/T 36363-2018.

There are two levels of porosity to keep apart: the separator as a whole and the coating are not the same thing. The coating has higher porosity, but that does not mean the wetting behaviour of the separator is decided by the coating alone — the electrolyte has to make its way through the full thickness path.

Air permeability is given in Gurley seconds, and a lower value means gas passes through more easily. Read together with porosity it forms the basis for wetting and transport capability, but the two do not substitute for each other: porosity describes space, permeability describes connectivity.

Why the two criteria have to be read together

High porosity and high permeability help wetting and ion transport, but the presence of gaps also reduces mechanical conformity against the electrode. Conversely, raising adhesion usually means a denser surface, which weakens wetting.

The company product performs on both at once: puncture strength retention reaches 40-60% in the 150 °C / 0.5 h window and still holds more than 20% in the 180 °C / 0.5 h window, while peel strength meets the >30 N/m criterion and separator porosity as a whole stays at about 35%-45%. These are coexisting conclusions, not alternatives.

So when a coated scheme is assessed, check adhesion and wetting as two separate boxes rather than asking one vague question about whether the interface is good.

Turning the interface conclusions into per-model checks

Work through them in order.

First, establish what the target cell demands for wetting (rate design and electrolyte system) and see whether the air permeability and porosity bands fall inside it. Second, confirm that the adhesion acceptance criterion matches your own requirement — that is the precondition for comparing anything side by side. Third, align the temperature band of the puncture strength retention with your duty rather than reading one figure on its own. Fourth, look at batch consistency: whether the supplier can give the distribution of peel strength and air permeability between batches.

The fourth step is the one most often skipped, and it is the one that decides whether a long-term cooperation can work. A single batch passing at sample stage and every batch landing in the same band in production are commitments of a different order.

A common misreading of the measurement basis

One point deserves separate mention: the porosity of the separator as a whole, the porosity of the coating, and air permeability are three different quantities, each with its own basis standard and method. Citing coating porosity as if it were separator porosity overstates the actual wetting and transport capability.

Stating the basis together with any figure is a quick way to judge whether a set of data is credible.