Semi-solid aramid-coated separators
Flagship productAn aramid coating layer is introduced on the separator surface for cell chemistries with high safety requirements, balancing high-temperature resistance, interface adhesion and mechanical retention after heat exposure.
- Six models on sale with total thickness of 9 / 11 / 13 / 14 µm, covering single-side, double-side and semi-solid structures
- Thermal shrinkage 1-2% (180 °C / 30 min); breakdown temperature above 400 °C
- Puncture strength retention after heat treatment: 40%-60% in the 150 °C / 0.5 h band, above 20% in the 180 °C / 0.5 h band
- Internal acceptance criterion for peel strength > 30 N/m (GB/T 7122-96)